Skip to main navigation Skip to search Skip to main content

110kV双回线路格构式复合材料杆塔的污秽性能

Translated title of the contribution: Pollution Performance of Lattice Composite Material Tower of 110 kV Double Circuit Line
  • 李 志军
  • , 陈 维江
  • , 姜 文东
  • , 王 灿灿
  • , 戴 敏
  • , 刘 宗喜
  • 华北电力大学电气与电子工程学院
  • 中国电力科学研究院
  • 国家电网公司
  • 国网浙江省电力公司
  • 国网浙江省电力公司丽水供电公司

Research output: Contribution to journal › Article › peer-review

4 Scopus citations

Abstract

Partial discharges happen at the heads of lattice composite material towers on 110 kV double circuit lines during pollution performance tests. In order to interpret and solve this unique phenomenon and problem, we demonstrated a typical design of lattice composite material towers for 110 kV double-circuit lines and conducted pollution performance tests of a designed full-scale test tower head. Significant partial discharges were observed around the steel caps of glass insulators and the metal bolts in nodes. Then we numerically calculated the distribution of electric field intensity and electric potential around the tower, and conducted additional relevant experiments to study the mechanism of partial discharges. The additional tests included power-frequency withstanding tests using contaminated tower head without spray wetting and pollution performance tests with protective measures applied to the meatal bolts, namely they were coated with room-temperature vulcanized silicon to increase the dielectric strength at their surfaces. It is obtained that, under the excitation of operating voltage on phase conductors, the electric potential distribute unevenly around the test tower head, for instance, the glass insulator string withstands a voltage of 49.7 kV, which is accounted for 50% of the test voltage. In the meantime, under the pollution test conditions including pollution and fog, discharge currents concentrate on the pollution layer of glass insulator strings(which perform relatively worse against pollution). Charges brought by these discharge currents gradually gather around the steel caps and metal bolts, improve the electric field intensity up to the critic value for starting coronas, and eventually lead to partial discharges. In conclusion, glass insulator strings with relatively worse pollution performance but withstanding high voltages are a fundamental source of partial discharges.Hence, a protective measure that substitutes anti-pollution composite insulators with strapping for glass insulator strings is proposed. Further tests have proved that using this measure can efficiently avoid the partial discharges in tower heads, and sustain the pollution flashover voltage of the true type test tower head up to 145 kV, possessing an adequate margin against pollution.
Translated title of the contributionPollution Performance of Lattice Composite Material Tower of 110 kV Double Circuit Line
Original languageChinese
Pages (from-to)1320-1327
Number of pages8
JournalGaodianya Jishu/High Voltage Engineering
Volume41
Issue number4
DOIs
StatePublished - 30 Apr 2015

Funding

国家电网公司重点科技项目(ZDK015-2011)~~;

Indexed by

  • EI
  • Scopus
  • CSCD

Fingerprint

Dive into the research topics of 'Pollution Performance of Lattice Composite Material Tower of 110 kV Double Circuit Line'. Together they form a unique fingerprint.

Cite this