Skip to main navigation Skip to search Skip to main content

Characterization of proton irradiation-induced defect in the A508-3 steel by slow positron beam

  • Qiang-mao Wan
  • , Guo-gang Shu
  • , Rong-shan Wang*
  • , Hui Ding
  • , Xiao Peng
  • , Qi Zhang
  • , Jing Lei
  • *Corresponding author for this work
  • Suzhou Nucl Power Res Inst Co Ltd

Research output: Contribution to journal › Article › peer-review

35 Scopus citations

Abstract

Proton irradiated A508-3 steel samples at room temperature were characterized by slow positron Doppler broadening spectroscopy to investigate the evolution of the irradiation-induced defects. S parameters of the irradiated samples were higher than those of the unirradiated samples. The S-W plot indicated that only one type of defect was presented in all the samples. These defects seem to be the vacancy-impurity complexes (associated with C, H, Mn or Ni) or divacancies. On the basis of the assumption that irradiation induced-defects consist of mono-vacancies, the concentration of these defects (similar to 10(20)/cm(3)) rapidly increases at the low dose (below about 0.15 dpa) and then tends to saturate at high dose (up to 0.35 dpa). (C) 2012 Elsevier B.V. All rights reserved.
Original languageEnglish
Pages (from-to)148-152
Number of pages5
JournalNuclear Instruments and Methods in Physics Research, Section B: Beam Interactions with Materials and Atoms
Volume287
DOIs
StatePublished - 15 Sep 2012

Funding

The authors would like to thank Dr. Ji Xia and Guang-Pu Wang Beijing Radiation Center, Beijing Normal University, Dr Wang Zhi-guang, institute of Modern Physics, Chinese Academy of Science, for their help with proton irradiations. The authors are grateful to Professor Yi-chu Wu, Wuhan university and Bao-yi Wang, Institute of High Energy Physics, Modern Physics, Chinese Academy of Science, for their help with slow positron Doppler broadening spectroscopy measurements. This work has been supported by National Science and Technology Major Project (No.2011ZX06004-002) and a grant from the National High Technology Research and Development Program of China (863 Program) (No. 2012AA050901). The work is also performed under the contract between China Guangdong Nuclear Power Holding Co., Ltd. (CGNPC) and Suzhou Nuclear Power Research Institute Co., Ltd. (SNPI) and the contact between Suzhou Nuclear Power Research Institute Co., Ltd. and Wuhan University.

Keywords

  • A508-3 steel
  • Ion irradiation
  • Slow positron beam

Indexed by

  • EI
  • Scopus
  • SCIE

Fingerprint

Dive into the research topics of 'Characterization of proton irradiation-induced defect in the A508-3 steel by slow positron beam'. Together they form a unique fingerprint.

Cite this