Creep fracture analysis of W strengthened 9%Cr steel weldment

  • Xue Wang*
  • , Qiangang Pan
  • , Zijun Liu
  • , Huiqiang Zeng
  • , Yongshun Tao
  • *Corresponding author for this work
  • Dongfang Boiler Grp Co Ltd

Research output: Chapter in Book/Report/Conference proceeding › Conference contribution › peer-review

Abstract

The creep rupture behaviour,hardness distribution and microstructure of weldment made y submerge arc welding for W strengthened P92 steel are described in this paper. The cross-weld Creep tests were carried out at 923K under stresses in the ranges 130-100MPa. For stress below 120MPa, weld-joints were ruptured by the Type IV crack, which located in their fine-grained heat affected zone(FGHAZ)with the smallest measured cross-weld hardness. A strong drop in creep rupture strength of weldment was induced by brittle type IV failure. In addition to coarsening of M23C6 carbides and an equiaxed fine grains in FGHAZ, intermetallic Fe-2(Mo,W)Laves phase precipitated on grain boundaries during creep is probably the significant factor caused the type IV failure.
Original languageEnglish
Title of host publicationMATERIALS PROCESSING TECHNOLOGIES, PTS 1 AND 2
PublisherTrans Tech Publications Ltd
Pages1699-1704
Number of pages2
ISBN (Print)978-0-87849-204-6, 9780878494033, 9780878499724, 9783037851234, 9783037851258, 9783037853566, 9783037855225, 9783037855942, 9783037856383, 9783037858257, 9783038351504
DOIs
StatePublished - Jan 2011

Publication series

NameAdvanced Materials Research
Volume154-155
ISSN (Print)1022-6680

Indexed by

  • CPCI-S
  • EI
  • Scopus

Fingerprint

Dive into the research topics of 'Creep fracture analysis of W strengthened 9%Cr steel weldment'. Together they form a unique fingerprint.

Cite this