Skip to main navigation Skip to search Skip to main content

Extra Bonding Layer Compensates Universal Adhesive's Thin Film Thickness

  • Mohammed H. Ahmed
  • , Chenmin Yao
  • , Kirsten Van Landuyt
  • , Marleen Peumans
  • , Bart Van Meerbeek*
  • *Corresponding author for this work
  • Univ Leuven
  • UZ Leuven
  • Tanta Univ

Research output: Contribution to journal › Article › peer-review

29 Scopus citations

Abstract

["Purpose: Universal adhesives (UAs) are applied in 2-step etch-and-rinse (2-E&R) or 1-step self-etch (1-SE) mode. This study investigated whether three UAs could benefit from a highly filled extra bonding layer (EBL), turning them into 3-E&R and 2-SE UAs, respectively, thus also compensating for the commonly thin film thickness of UAs.","Materials and Methods: Microtensile bond strength (mu TBS) to bur-cut dentin of Clearfil Universal Bond Quick (C-UBq; Kuraray Noritake), G-Premio Bond (G-PrB; GC) and Prime&Bond Active (P & Ba; Dentsply Sirona), applied in E&R and SE mode without/with the adhesive resin (EBL) of OptiBond FL (Opti-FL_ar; Kerr), was compared to that of the 3-E& Ra OptiBond FL (Opti-FL; Kerr), which was also employed in 2-SE mode. As a cross reference, the SE primer of Clearfil SE Bond 2 (Kuraray Noritake) was combined with Opti-FL_ar (C-SE2/Opti-FL) and again applied in 2-SE and 3-E&R mode. mu TBS was measured after 1 month of water storage (37 degrees C) and additional 25,000 and 50,000 thermocycles (TC). All mu TBS were statistically analyzed using three different linear mixed-effects models with specific contrasts (p < 0.05).","Results: Overall, the four parameters (adhesive, bonding mode, aging, EBL) significantly influenced mu TBS. G-PrB and P&Ba benefited from EBL when applied in both E&R and SE bonding modes. In E&R mode, P&Ba generally revealed the highest mu TBS; C-UBq presented an intermediate and G-PrB the lowest mu TBS. No significant differences were found between different bonding modes. C-SE2/Opti-FL outperformed Opti-FL in 3-E&R and 2-SE_1 month/25k.","Conclusion: The overall benefit of EBL on the 1-month and TC-aged bonding efficacy differed for the different UAs tested."]
Original languageEnglish
Pages (from-to)483-501
Number of pages19
JournalJournal of Adhesive Dentistry
Volume22
Issue number5
DOIs
StatePublished - Sep 2020

Funding

MHA was appointed as PhD researcher at KU Leuven -BIOMAT, based on funding provided by the Ministry of Higher Education of Egypt. The companies Dentsply Sirona, GC, Kuraray Noritake and Kerr are gratefully acknowledged for providing the materials employed and investigated.

Keywords

  • bond strength
  • durability
  • hydrophobic
  • linear mixed model (LME)
  • adhesive-dentin interface

Indexed by

  • Scopus
  • SCIE

Fingerprint

Dive into the research topics of 'Extra Bonding Layer Compensates Universal Adhesive's Thin Film Thickness'. Together they form a unique fingerprint.

Cite this