Skip to main navigation Skip to search Skip to main content

Fabrication of TiAl nano-alloy by mechanical activation-spark plasma sintering process in situ

  • Zhi-Wei Wang
  • , Yu-Xiang Shi

Research output: Contribution to journal › Article › peer-review

Abstract

Powder of (Ti-50at%Al)-10wt%Al2O3 was get through ball milling mechanical activation (MA), and then sintered and concurrently consolidated by using spark plasma sintering (SPS) process. TiAl-Al2O3 bulk nano-material was fabricated using the method of mechanical activation-spark plasma sintering (MA-SPS) in situ. The original and ball milled (Ti-50at%Al)-10wt%Al2O3 showed similar X-ray diffraction profiles. After MA, the crystal sizes of nano-powder are less than 25 nm. Al2O3 has effect of mechanical activation, while makes crystal fine and accelerates nano-process. The nano-powder was sintered into TiAl alloy on a temperature lower than 800°C, and for a sintering time less than 5 min. The microstructure of TiAl alloy contains gamma TiAl and alpha-2 Ti3Al phase. Through SPS in situ, the final nano-material has dual-phase (γ+α2), and its density is 3.73 g/cm3. The crystal sizes of dual-phase are less than 130 nm.
Original languageEnglish
Pages (from-to)1794-1797
JournalGongneng Cailiao/Journal of Functional Materials
Volume36
Issue number11
StatePublished - Nov 2005

Indexed by

  • EI

Fingerprint

Dive into the research topics of 'Fabrication of TiAl nano-alloy by mechanical activation-spark plasma sintering process in situ'. Together they form a unique fingerprint.

Cite this