Abstract
Wafer probe testing is essential for evaluating the reliability of microelectronic devices. As device dimensions continue to shrink, the mechanical stress at the probe tip increases the risk of failure occurring in the brittle dielectric layer. Existing studies usually simplify the plastic behavior of bond pads in finite element (FE) models, making it difficult to accurately predict the stress in the dielectric layer. In this study, the FE model for wafer probe testing was improved by implanting the true plastic properties of Al-(4 wt.%)Cu bond pads obtained from nanoindentation inverse identification. Specifically, a MATLAB and ABAQUS co-simulation method is employed to inversely obtain the plastic properties of Al-(4 wt.%)Cu bond pads from the nanoindentation load-displacement curve. By comparing different gradient-based optimization algorithms, the Levenberg-Marquardt (LM) algorithm was found to be the most suitable for balancing computational efficiency and accuracy in inverse identification. Moreover, a hybrid optimization strategy combining Gauss-Newton and LM algorithms is proposed to mitigate sensitivity to initial values. The results show that the improved model of wafer probe testing achieves high accuracy in stress prediction. This study provides a high-fidelity approach for mechanical reliability assessment of wafer probe testing.
| Translated title of the contribution | 基于纳米压痕反演识别的晶圆探针测试力学建模 |
|---|---|
| Original language | English |
| Article number | 425545 |
| Number of pages | 14 |
| Journal | Acta Mechanica Sinica/Lixue Xuebao |
| Volume | 42 |
| Issue number | 7 |
| Early online date | May 2026 |
| DOIs | |
| State | Published - 4 May 2026 |
Funding
This work was supported by the National Key R&D Program of China (Grant No. 2022YFB3207100), National Natural Science Foundation of China (Grant No. L2424216), and Major Program (JD) of Hubei Province (Grant No. 2023BAA008).
Indexed by
- SCIE
- Scopus
Fingerprint
Dive into the research topics of 'Mechanical modeling of wafer probe testing based on nanoindentation inverse identification'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver