Skip to main navigation Skip to search Skip to main content

Microstructure and nanoindentation analyses of low-temperature aging on the zirconia-porcelain interface

  • M. D. Peng
  • , J. Q. Wei
  • , Y. N. Wang*
  • , Q. Li*
  • *Corresponding author for this work

Research output: Contribution to journal › Article › peer-review

9 Scopus citations

Abstract

The aim of the present study was to investigate the effects of low-temperature aging on the micro-mechanical and micro-structural properties of zirconia-porcelain interface. In total, thirty-three Y-TZP zirconia blocks were fabricated by using CAD/CAM technology, veneered with porcelains. Specimens were submitted to low temperature aging in an autoclave at 134 degrees C, additional 0.2 MPa pressure for 0 h, 5 h, or 10 h. Flexural strength was obtained by using three-point bending test. Micro-mechanical properties (nano-hardness (H) and reduced modulus (Er)) were investigated by nanoindentation tests. Scanning electron microscopy and X-ray diffraction analyses were performed to identify the micro-structure and fracture behavior. The flexure strength, modulus and hardness of zirconia increased after 5 h aging and decreased after 10 h aging. No significant alterations of the reduced modulus or hardness of porcelain were detected in the whole aging duration. Width of the zirconia-porcelain interface was extended towards the bulk of zirconia. The detachment and cracks could be observed in zirconia, and the crystal alignment was disorganized in porcelain after 5 h aging and 10 h aging. Mechanical properties of the veneering porcelain are not affected by low-temperature aging. However, the expansion and the alterations of micro-mechanical and micro-structural properties of zirconia-porcelain interface were detected.
Original languageEnglish
Pages (from-to)119-126
Number of pages8
JournalJournal of the Mechanical Behavior of Biomedical Materials
Volume66
DOIs
StatePublished - Feb 2017

Funding

This study was supported by grants from Hubei Province Health and Family Planning Scientific Research Project (No. WJ2015Q025).

Keywords

  • Zirconia-based restorations
  • Low-temperature aging
  • Zirconia-porcelain interface
  • Nanoindentation
  • Flexural strength

Indexed by

  • EI
  • Scopus
  • SCIE

Fingerprint

Dive into the research topics of 'Microstructure and nanoindentation analyses of low-temperature aging on the zirconia-porcelain interface'. Together they form a unique fingerprint.

Cite this