TY - JOUR
T1 - Self-assembly of chitosan and cellulose chains into a 3D porous polysaccharide alloy films: Co-dissolving, structure and biological properties
AU - Zhang, Ruihong
AU - Xie, Jinyu
AU - Yang, Binbin
AU - Fu, Feiya
AU - Tang, Haiyue
AU - Zhang, Jingjing
AU - Zhao, Yanteng
AU - Zhang, Yanyan
AU - Liu, Lin
AU - Zhu, Yaofeng
AU - Liu, Xiangdong
AU - Zhou, Jinping
AU - Yao, Juming
PY - 2019/11/1
Y1 - 2019/11/1
N2 - Blending of plant-based cellulose and marine-derived chitosan in micro-level has potential to make fascinating materials. However, this task is frequently hindered by the poor solubility of the polysaccharides. Here, using a green alkali/urea solvent media together with a well-designed dissolving strategy, original cellulose pulp and chitosan power were dispersed into a homogeneous solution. Driven by the intermolecular hydrogen-bond interaction, cellulose and chitosan chains were facially self-assembled into a unique 3D alloy structure. Owing to the rich interface interactions, the tensile strength and breaking elongation of the alloy film increased by 69% and 260%, respectively, when compared to a pure chitosan film. Besides, the 3D alloy films with a pore diameter of 920-1435 nm exhibited an extremely high cell viability which was higher than 95%. Additionally, accelerated wound healing rate of 95.6% reached in the presence of the alloy film after two weeks using a full-thickness wound in a rat model.
AB - Blending of plant-based cellulose and marine-derived chitosan in micro-level has potential to make fascinating materials. However, this task is frequently hindered by the poor solubility of the polysaccharides. Here, using a green alkali/urea solvent media together with a well-designed dissolving strategy, original cellulose pulp and chitosan power were dispersed into a homogeneous solution. Driven by the intermolecular hydrogen-bond interaction, cellulose and chitosan chains were facially self-assembled into a unique 3D alloy structure. Owing to the rich interface interactions, the tensile strength and breaking elongation of the alloy film increased by 69% and 260%, respectively, when compared to a pure chitosan film. Besides, the 3D alloy films with a pore diameter of 920-1435 nm exhibited an extremely high cell viability which was higher than 95%. Additionally, accelerated wound healing rate of 95.6% reached in the presence of the alloy film after two weeks using a full-thickness wound in a rat model.
KW - Alkali/urea solvent
KW - Co-dissolution
KW - Polysaccharide alloy
KW - Physicochemical properties
KW - Wound-healing
KW - Alkali/urea solvent
KW - Co-dissolution
KW - Polysaccharide alloy
KW - Physicochemical properties
KW - Wound-healing
UR - https://openir.whu.edu.cn/AchievementDetail/WOS_b6325ebf-7080-4581-a614-1e26785d76d6
U2 - 10.1016/j.apsusc.2019.06.193
DO - 10.1016/j.apsusc.2019.06.193
M3 - Article
SN - 0169-4332
VL - 493
SP - 1032
EP - 1041
JO - Applied Surface Science
JF - Applied Surface Science
ER -