摘要
The erosion-corrosion of aluminum in a 50 degrees C ethylene glycol aqueous solution (EGAS) was studied. Compared with that in deionized water, the corrosion of aluminum in an EGAS was inhibited to a certain extent. The corrosion potential, corrosion current, and charge transfer impedance of aluminum changed from -1.5776 V, 380.4 nA cm(-2), and 1.924 x 10(-4) omega cm(-2) in deionized water to -1.3127 V, 285.5 nA cm(-2), and 4.041 x 10(-4) omega cm(-2) in a 45.3 vt% EGAS, respectively. Ethylene glycol did not ionize in deionized water and the ionic conductivity of the EGAS was low, effectively restraining the corrosion of aluminum. However, a test with aluminum in an EGAS after long-term storage (9 days) showed that ethylene glycol gradually oxidized to glycolic acid, oxalic acid, and other substances, which slowly corroded the aluminum surface. Analysis results showed that the corrosion products on the surface of aluminum were Al(OH)(3) and Al2O3. The pitting hole formation mechanism of aluminum occurs via an aluminum-alcohol phase formed on the aluminum surface, which can inhibit the dissolution of the oxide film. Therefore, a suitably concentrated EGAS with a high heat capacity and low ionic conductivity similar to that of deionized water can be used as a coolant in airtight valve cooling systems for high-voltage direct-current transmission.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 1899-1907 |
| 页数 | 9 |
| 期刊 | Materials and Corrosion |
| 卷 | 72 |
| 期 | 12 |
| 早期在线日期 | 8月 2021 |
| DOI | |
| 出版状态 | 已出版 - 12月 2021 |
基金资助
Programs of the China Southern Power Grid, Grant/Award Numbers: CGYKJXM20180229, 20180405
关键词
- aluminum
- erosion-corrosion
- ethylene glycol
- high-voltage direct-current transmission
- radiator
收录
- EI
- Scopus
- SCIE
学术指纹
探究 'Erosion-corrosion behavior of aluminum in a 50°C ethylene glycol aqueous solution simulating cooling water in HVDC transmission' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver