Positron lifetime spectra in polybutadiene (PB) have been measured in the temperature range 95-305K. By analyzing the analogy of the temperature-dependent the o-Ps intensity I3 in polypropylene (PP), high and low density polyethylene (HDPE, LDPE), we propose that above the glass transition temperature Tg the o-Ps intensity I3 shows the scaling relation I3 approx. (T-Tg)beta. The data indicate the existence of a crossover temperature Tc, located above Tg, where the β value changes greatly; and that of an excluding temperature Te beyond which o-Ps lifetime τ3 is saturated. When Tgc, β has the order of magnitude of 10-2. When Tc&leTe, β =0.267 ± 0.01 is identical for linear polymers PB, PP and LDPE, while β = 0.434 ± 0.02 for the branched LDPE. Based on the lattice model of polymers, the curves of the hole formation energy vs temperature are calculated and show analogous for the four polymers. These results reveal a common feature of hole creation above Tg in polymers.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 797-800 |
| 期刊 | Materials Science Forum |
| 卷 | 175-178 |
| 期 | pt 2 |
| 出版状态 | 已出版 - 1月 1995 |
关键词
- Polybutadienes
收录
- EI
学术指纹
探究 'Scaling behaviour and formation energy of free-volume in polymers probed by positron annihilation' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver